Not every “heat-resistant” glove is the same glove.
We see this a lot in PPE catalogs: one rating, applied to everything from TIG welding to foundry work.
But heat protection under EN 407 is measured in six separate tests —
and a glove that excels at one is often mediocre at another.
The six EN 407 tests
- Burning behaviour — does the material keep burning after ignition?
- Contact heat — how long before the inside temperature rises 15°C?
- Convective heat — resistance to flame exposure.
- Radiant heat — heat coming off a hot surface without direct contact.
- Small splashes of molten metal — the everyday risk in MIG and stick welding.
- Large quantities of molten metal — foundry, casting, steel pouring.
Each test is graded separately, usually 0 to 4. A marking such as
EN 407: 413X4X is not a single “heat level” — it is six answers,
and the X means that particular test was not performed.
Put it in a foundry and you have sold your customer a problem, not protection.
Match the rating to the actual operation
| Operation | What actually matters | Typical construction |
|---|---|---|
| TIG welding | Dexterity and moderate heat. Low spatter, but the operator needs to feel the torch and filler rod. | Thin goatskin or grain leather, light lining, snug cuff. |
| MIG / stick welding | Splash resistance. Small molten metal splashes are the daily risk, plus radiant heat from the arc. | Cow split leather, reinforced palm, cotton or aramid lining, longer cuff. |
| Foundry / casting / pouring | The highest molten-metal grade. Large quantities of molten metal, not just droplets. | Heavy split leather, thick heat-barrier lining, long gauntlet, quick-release design. |
Specifying one glove for all three is how catalogs go wrong. The TIG glove is too thin for a foundry;
the foundry glove is far too clumsy for TIG.
Keep leather thickness and lining honest
Heat resistance is built into the material, not the label. Two things decide it:
- Leather grade and thickness — we specify thickness per model, typically 1.0–1.4 mm
for welding gloves, heavier for foundry work. A glove marked with a high EN 407 grade but made from thin
split will not repeat that result batch after batch. - Lining — cotton, brushed acrylic, aramid or aluminised layers each behave differently
under contact versus radiant heat. The lining is part of the tested construction, so changing it changes the rating.
If a supplier cannot tell you the leather thickness and the lining composition, the rating on the
datasheet is not something you can rely on.
Send the EN 407 test report with the offer, item by item
We attach the test report for each model we quote — not one generic certificate covering the whole range.
The report should show:
- The six individual EN 407 grades, not a summary score
- The tested construction (leather type, thickness, lining)
- The accredited laboratory and report number
That way your customer can check the glove against their own risk assessment, and you are not
guessing when a safety officer asks for evidence.
A quick note on EN 388
Heat is only half the picture. EN 388 covers mechanical risks: abrasion, blade cut,
tear and puncture, plus the ISO 13997 cut level (letters A to F) and an impact mark P
when the glove passes impact testing.
For sheet metal, glass and blade handling, the ISO cut letter is usually the number that matters most,
because the older blade-cut test saturates on high-performance fibres. Our A5 cut-resistant gloves are
specified on that letter, not on the older blade-cut number.
A glove can be excellent for welding and still be a poor choice for glass handling —
the two standards answer different questions.
How to specify in an inquiry
Send us four things and we will come back with a construction and the matching test report:
- The operation — TIG, MIG/stick, foundry, cutting, assembly
- The working temperature range and whether molten metal is involved
- The dexterity the operator needs
- The target cost per pair and annual volume
We make welding gloves, A5 cut-resistant gloves and heat-resistant gloves for distributors across
the Middle East, Russia, Central Asia and Europe — and we would rather help you
spec it right than ship it twice.
Send us your operation details and we will reply within 12 hours
with a specification sheet, the EN 407 / EN 388 report and a quotation.